Docs › Examples › Rate capability of a lithium-ion cell

Electrochemistry · 1D

Rate capability of a lithium-ion cell

A 5 Ah graphite-SiOx | NMC811 cell discharged at six rates from C/10 to 1.5C, and why its electrolyte sets the limit.

Doyle-Fuller-NewmanRate capabilityLimiting currentPeukert

Run locally with OneSimulation. The example downloads are free. Running them requires an activated runtime. OneSimulation 1.0 · CPython 3.13 on macOS (Apple Silicon), Ubuntu 22.04 (x86-64), and Windows x64. Installation and activation · View pilot plans. Scope of the reference checks.

Rate capability of a lithium-ion cell
Rate capability of a lithium-ion cell. Run the notebook to produce its own figures.

What it computes

OneSimulation solves the Doyle-Fuller-Newman porous-electrode model through the cell thickness for each constant-current discharge and reads capacity and energy at the 2.5 V cut-off. The salt depletion of the electrolyte is compared with the steady salt balance, which gives the limiting current of the cell.

What it checks

Capacity falls from 5.081 Ah at C/10 (99.8 % of the stoichiometric 5.090 Ah) to 4.854 Ah at 1.5C and energy from 18.77 to 16.59 Wh (Peukert exponent 1.028); the minimum salt concentration follows the steady balance c0(1 - I/I_lim) within 2.5 to 30 mol/m³, with a limiting current of 9.8 A (1.96C).

The notebook

The complete notebook, cell by cell. Run it to produce the figures and the comparison printout.

The faster a cell is discharged, the larger its polarisation, the earlier it reaches the cut-off voltage and the less capacity and energy it delivers. In a cell with thick, dense electrodes the electrolyte is often the bottleneck: lithium salt is produced in the negative electrode and consumed in the positive one, and the salt concentration near the positive collector falls.

For a uniform reaction rate the steady salt balance \(-D_e\,c_e'=(1-t_+)\,i_e/F\) with an ionic current rising linearly from zero to \(I\) in the negative electrode, constant in the separator and falling back to zero in the positive electrode gives

\[c_e(x)=c_0+\frac{(1-t_+)\,I}{F}\big(\bar g-g(x)\big),\qquad g(x)=\int_0^x\frac{i_e/I}{D_e}\,dx,\]

where \(\bar g\) is the porosity-weighted mean of \(g\) that conserves the salt. The concentration reaches zero at the positive collector at the limiting current \(I_\mathrm{lim}=F c_0/\big((1-t_+)(g(L)-\bar g)\big)\), so the minimum concentration falls as \(c_0(1-I/I_\mathrm{lim})\).

Reference. Cell parameters of Chen et al., J. Electrochem. Soc. 167 (2020) 080534 (LG M50, 5 Ah); model of Doyle, Fuller and Newman, J. Electrochem. Soc. 140 (1993) 1526. Checks: (i) at low rate the delivered capacity approaches the stoichiometric capacity of the limiting electrode; (ii) the electrolyte follows the steady salt balance and the limiting current above; (iii) the capacity-rate data are summarised by Peukert's law \(Q\propto I^{1-k}\).

import numpy as np
from onesim.physics.chemistry import (
    BatteryElectrodeLayer,
    BatteryElectrolyteLayer,
    PorousElectrodeBattery,
)
from onesim.visualization import plots, theme

theme.set()

Cell

faraday, area, transference = 96485.33212, 0.1027, 0.2594
negative_ocp = lambda x, T: (
    1.9793 * np.exp(-39.3631 * x)
    + 0.2482
    - 0.0909 * np.tanh(29.8538 * (x - 0.1234))
    - 0.04478 * np.tanh(14.9159 * (x - 0.2769))
    - 0.0205 * np.tanh(30.4444 * (x - 0.6103))
)
positive_ocp = lambda y, T: (
    4.4875
    - 0.8090 * y
    - 0.0428 * np.tanh(18.5138 * (y - 0.5542))
    - 17.7326 * np.tanh(15.7890 * (y - 0.3117))
    + 17.5842 * np.tanh(15.9308 * (y - 0.3120))
)
negative = BatteryElectrodeLayer(
    thickness=85.2e-6,
    porosity=0.25,
    electrolyte_diffusivity=1.7694e-10 * 0.25**1.5,
    electrolyte_conductivity=0.9487 * 0.25**1.5,
    particle_radius=5.86e-6,
    particle_diffusivity=3.3e-14,
    active_fraction=0.75,
    maximum_concentration=33133,
    initial_stoichiometry=0.9014,
    reference_exchange_current=6.48e-7 * np.sqrt(1000) * 33133 / 2,
    electronic_conductivity=215,
    open_circuit_potential=negative_ocp,
)
positive = BatteryElectrodeLayer(
    thickness=75.6e-6,
    porosity=0.335,
    electrolyte_diffusivity=1.7694e-10 * 0.335**1.5,
    electrolyte_conductivity=0.9487 * 0.335**1.5,
    particle_radius=5.22e-6,
    particle_diffusivity=4e-15,
    active_fraction=0.665,
    maximum_concentration=63104,
    initial_stoichiometry=0.2661,
    reference_exchange_current=3.42e-6 * np.sqrt(1000) * 63104 / 2,
    electronic_conductivity=0.18,
    open_circuit_potential=positive_ocp,
)
separator = BatteryElectrolyteLayer(
    thickness=12e-6,
    porosity=0.47,
    electrolyte_diffusivity=1.7694e-10 * 0.47**1.5,
    electrolyte_conductivity=0.9487 * 0.47**1.5,
)
cell = PorousElectrodeBattery(
    negative=negative,
    separator=separator,
    positive=positive,
    electrolyte_concentration=1000,
    transference_number=transference,
)
stoichiometric = faraday * 0.75 * 85.2e-6 * 33133 * (0.9014 - 0.0279) * area / 3600

Discharges

Each discharge starts from the full cell and runs a little past the 2.5 V cut-off (the end time is given as a fraction of the nominal hour count); the capacity is read at the cut-off.

rates = {0.1: 1.02, 0.2: 1.02, 0.5: 1.01, 1.0: 0.995, 1.25: 0.985, 1.5: 0.972}
runs = {
    rate: cell.solve(
        mode="DFN",
        current_density=5.0 * rate / area,
        final_time=end * 3600 / rate,
        radial_cells=12,
        through_cells=(8, 4, 8),
        output_times=np.linspace(0, end * 3600 / rate, 800),
    )
    for rate, end in rates.items()
}

Results

layers = (
    (negative, 0.0),
    (separator, negative.thickness),
    (positive, negative.thickness + separator.thickness),
)
x = np.linspace(0, negative.thickness + separator.thickness + positive.thickness, 4001)
g = lambda x: np.where(
    x < negative.thickness,
    x**2 / (2 * negative.thickness * negative.electrolyte_diffusivity),
    np.where(
        x < layers[2][1],
        negative.thickness / (2 * negative.electrolyte_diffusivity)
        + (x - negative.thickness) / separator.electrolyte_diffusivity,
        g_end
        - (x[-1] - x) ** 2
        / (2 * positive.thickness * positive.electrolyte_diffusivity),
    ),
)
g_end = (
    negative.thickness / (2 * negative.electrolyte_diffusivity)
    + separator.thickness / separator.electrolyte_diffusivity
    + positive.thickness / (2 * positive.electrolyte_diffusivity)
)
porosity = np.select(
    [x < negative.thickness, x < layers[2][1]],
    [negative.porosity, separator.porosity],
    positive.porosity,
)
g_mean = np.trapezoid(porosity * g(x), x) / np.trapezoid(porosity, x)
limiting = faraday * 1000 / ((1 - transference) * (g_end - g_mean))
results = {}
for rate, run in runs.items():
    capacity = 5.0 * rate * run.times / 3600
    cut = np.argmax(run.terminal_voltage < 2.5)
    q = np.interp(
        2.5, run.terminal_voltage[cut : cut - 2 : -1], capacity[cut : cut - 2 : -1]
    )
    keep = capacity <= q
    results[rate] = dict(
        q=q,
        energy=np.trapezoid(run.terminal_voltage[keep], capacity[keep]),
        salt=run.electrolyte_concentration[keep].min(),
        profile=run.electrolyte_concentration[np.flatnonzero(keep)[-1]],
    )
peukert = (
    1
    - np.polyfit(
        np.log(list(rates)[2:]), np.log([results[r]["q"] for r in list(rates)[2:]]), 1
    )[0]
)
print(
    f"stoichiometric capacity of the negative electrode {stoichiometric:.4f} Ah; limiting current of the steady salt balance "
    f"{limiting:.1f} A/m² = {limiting * area:.2f} A = {limiting * area / 5:.2f}C"
)
print(
    "C-rate   capacity [Ah]  of stoichiometric   energy [Wh]   mean voltage [V]   min salt [mol/m³]   steady balance c0(1-I/I_lim)"
)
for rate, r in results.items():
    print(
        f"{rate:6.2f}   {r['q']:12.4f}   {100 * r['q'] / stoichiometric:13.1f} %   {r['energy']:11.3f}   {r['energy'] / r['q']:15.4f}"
        f"   {r['salt']:17.1f}   {1000 * (1 - 5 * rate / area / limiting):17.1f}"
    )
print(f"Peukert exponent from C/2 to 1.5C: k = {peukert:.4f}")

Figure

Discharge curves, capacity and energy over the rate, the salt profile at the cut-off against the steady balance, and the minimum salt concentration on its way to the limiting current.

fig = plots.figure(2, 2, size=(14, 10))
plots.line(
    y={
        f"{rate:g}C": (5.0 * rate * run.times / 3600, run.terminal_voltage)
        for rate, run in runs.items()
    },
    hlines={"cut-off": 2.5},
    xlimits=(0, 5.3),
    ylimits=(2.4, 4.25),
    xlabel="discharged capacity [Ah]",
    ylabel="terminal voltage [V]",
    title="Discharge curves from C/10 to 1.5C",
    legend="lower left",
    ax=fig[0],
)
plots.line(
    list(rates),
    {"capacity [Ah]": [r["q"] for r in results.values()]},
    right={"energy [Wh]": [r["energy"] for r in results.values()]},
    hlines={"stoichiometric capacity": stoichiometric},
    ylimits=(4.82, 5.12),
    markers=True,
    scale="logx",
    xlabel="C-rate",
    ylabel="capacity to 2.5 V [Ah]",
    right_label="energy to 2.5 V [Wh]",
    title="Rate capability",
    legend="lower left",
    ax=fig[1],
)
plots.line(
    1e6 * runs[0.1].electrolyte_positions,
    {f"{rate:g}C": r["profile"] for rate, r in results.items() if rate >= 0.5},
    reference={
        f"{rate:g}C": (
            1e6 * x,
            1000 + (1 - transference) * 5 * rate / area / faraday * (g_mean - g(x)),
        )
        for rate in results
        if rate >= 0.5
    },
    vlines=[1e6 * negative.thickness, 1e6 * layers[2][1]],
    xlabel="x [µm]",
    ylabel="salt concentration [mol/m³]",
    title="Salt at the cut-off, dashed: steady balance",
    legend="lower left",
    ax=fig[2],
)
plots.line(
    points={
        "simulation": (
            5 * np.array(list(rates)) / area,
            [r["salt"] for r in results.values()],
        )
    },
    reference={
        "steady balance c₀(1 - I/I_lim)": (
            np.linspace(0, limiting, 50),
            1000 * (1 - np.linspace(0, limiting, 50) / limiting),
        )
    },
    vlines={"limiting current": limiting},
    xlabel="current density [A/m²]",
    ylabel="minimum salt concentration [mol/m³]",
    title="Towards the limiting current",
    legend="upper right",
    ax=fig[3],
)
plots.show()

Going further

Thinner or more porous electrodes raise the limiting current: change the thickness and porosity and see the rate capability improve at the expense of the stored energy per area.