"""OneSimulation example: lithium-ion cell with a single-ion conducting electrolyte in 1D.
Requires the installed, activated OneSimulation runtime.

In a single-ion conductor only the lithium ions move (transference number one): no salt
concentration gradient builds up and the electrolyte acts as a pure ionic resistor. The porous
electrode model of the cell is discharged at several rates and electrolyte conductivities. The salt
concentration is checked to stay uniform, the well-conducting limit against the single-particle
model, and the voltage shift with the conductivity against the ohmic resistance of the layers.
"""

# # Lithium-ion cell with a single-ion conducting electrolyte
#
# Liquid electrolytes carry the current with both ions; the anions pile up at one electrode and
# deplete at the other, and the salt gradient limits the rate. Polymer and ceramic single-ion
# conductors fix the anions to the host, so the lithium transference number is $t_+=1$. In the
# porous electrode (Doyle-Fuller-Newman) model the salt balance then has no source,
#
# $$\varepsilon\frac{\partial c_e}{\partial t}=\nabla\cdot\big(D_\mathrm{eff}\nabla c_e\big)+(1-t_+)\frac{a\,j}{F}
#   \quad\Rightarrow\quad c_e=c_{e,0},$$
#
# and the ionic current obeys Ohm's law, $i_e=-\kappa_\mathrm{eff}\nabla\phi_e$, without the diffusion
# potential $\propto(1-t_+)\nabla\ln c_e$. The electrodes, particles and kinetics are those of the
# LG M50 cell (graphite-SiOx | NMC811, 5 Ah, 25 °C) of Chen et al., *J. Electrochem. Soc.* 167
# (2020) 080534; the electrolyte is replaced by a single-ion conductor of bulk conductivity
# $\kappa$ = 1, 0.3 and 0.1 S/m with the Bruggeman correction $\kappa_\mathrm{eff}=\kappa\varepsilon^{1.5}$.
#
# **Reference.** (i) The salt concentration must stay at its initial value. (ii) For very high
# ionic and electronic conductivities the reaction is uniform through each electrode and the model
# reduces exactly to the single-particle model (SPM). (iii) If the reaction stayed uniform through
# the electrodes, lowering the conductivity would shift the voltage by the ohmic drop
# $\Delta V=i\,\Delta R$ with $R=\frac{L_-}{3\kappa_{\mathrm{eff},-}}+\frac{L_s}{\kappa_{\mathrm{eff},s}}+\frac{L_+}{3\kappa_{\mathrm{eff},+}}$,
# the classical one-third rule of a porous electrode with uniform reaction (J. Newman, K.E.
# Thomas-Alyea, *Electrochemical Systems*, 3rd ed., Wiley 2004, §22). It is the limit for a weak
# resistance and an upper bound otherwise, because a poorer conductor pulls the reaction towards
# the separator and shortens the ionic path.

import numpy as np
from onesim.physics.chemistry import (
    BatteryElectrodeLayer,
    BatteryElectrolyteLayer,
    PorousElectrodeBattery,
)
from onesim.visualization import plots, theme

theme.set()

# ## Cell
#
# The layers of the LG M50 cell; only the electrolyte conductivity changes. The salt diffusivity
# no longer matters at $t_+=1$ and is kept at the liquid value.

faraday, area = 96485.33212, 0.1027
negative_ocp = lambda x, T: (
    1.9793 * np.exp(-39.3631 * x)
    + 0.2482
    - 0.0909 * np.tanh(29.8538 * (x - 0.1234))
    - 0.04478 * np.tanh(14.9159 * (x - 0.2769))
    - 0.0205 * np.tanh(30.4444 * (x - 0.6103))
)
positive_ocp = lambda y, T: (
    4.4875
    - 0.8090 * y
    - 0.0428 * np.tanh(18.5138 * (y - 0.5542))
    - 17.7326 * np.tanh(15.7890 * (y - 0.3117))
    + 17.5842 * np.tanh(15.9308 * (y - 0.3120))
)
porosity = {"negative": 0.25, "separator": 0.47, "positive": 0.335}
thickness = {"negative": 85.2e-6, "separator": 12e-6, "positive": 75.6e-6}
cell = lambda kappa, sigma=None: PorousElectrodeBattery(
    negative=BatteryElectrodeLayer(
        thickness=thickness["negative"],
        porosity=porosity["negative"],
        electrolyte_diffusivity=1.7694e-10 * 0.25**1.5,
        electrolyte_conductivity=kappa * 0.25**1.5,
        particle_radius=5.86e-6,
        particle_diffusivity=3.3e-14,
        active_fraction=0.75,
        maximum_concentration=33133,
        initial_stoichiometry=0.9014,
        reference_exchange_current=6.48e-7 * np.sqrt(1000) * 33133 / 2,
        electronic_conductivity=sigma or 215,
        open_circuit_potential=negative_ocp,
    ),
    separator=BatteryElectrolyteLayer(
        thickness=thickness["separator"],
        porosity=porosity["separator"],
        electrolyte_diffusivity=1.7694e-10 * 0.47**1.5,
        electrolyte_conductivity=kappa * 0.47**1.5,
    ),
    positive=BatteryElectrodeLayer(
        thickness=thickness["positive"],
        porosity=porosity["positive"],
        electrolyte_diffusivity=1.7694e-10 * 0.335**1.5,
        electrolyte_conductivity=kappa * 0.335**1.5,
        particle_radius=5.22e-6,
        particle_diffusivity=4e-15,
        active_fraction=0.665,
        maximum_concentration=63104,
        initial_stoichiometry=0.2661,
        reference_exchange_current=3.42e-6 * np.sqrt(1000) * 63104 / 2,
        electronic_conductivity=sigma or 0.18,
        open_circuit_potential=positive_ocp,
    ),
    electrolyte_concentration=1000,
    transference_number=1.0,
)
resistance = lambda kappa: sum(
    thickness[n] / ((1 if n == "separator" else 3) * kappa * porosity[n] ** 1.5)
    for n in thickness
)
print(
    "ohmic resistance of the electrolyte, uniform reaction: "
    + ", ".join(
        f"kappa = {k:g} S/m: {resistance(k) * 1e4:.2f} Ohm cm²" for k in (1.0, 0.3, 0.1)
    )
)

# ## Discharges
#
# Each discharge covers 80 % of the nominal capacity at 0.5C and 1C, for the three conductivities,
# with the full porous electrode model. A fourth run at 1C with conductivities of $10^3$ S/m in
# both phases is compared with the single-particle model.

one_c = 5.0 / area
runs = {
    (kappa, rate): cell(kappa).solve(
        mode="DFN",
        current_density=rate * one_c,
        final_time=0.8 * 3600 / rate,
        radial_cells=16,
        through_cells=(10, 5, 10),
        output_times=np.linspace(0, 0.8 * 3600 / rate, 241),
    )
    for kappa in (1.0, 0.3, 0.1)
    for rate in (0.5, 1.0)
}
ideal = cell(1e3, sigma=1e3)
limit = {
    mode: ideal.solve(
        mode=mode,
        current_density=one_c,
        final_time=0.8 * 3600,
        radial_cells=16,
        through_cells=(10, 5, 10),
        output_times=np.linspace(0, 0.8 * 3600, 241),
    )
    for mode in ("DFN", "SPM")
}

# ## Comparison with the references
#
# The largest relative deviation of the salt concentration from 1000 mol/m³, the high-conductivity
# model against the SPM, and the voltage shift at the first output time (12 s at 1C) against the
# ohmic estimate.

print(
    f"largest |c_e - c_e0| / c_e0 over all runs: {max(np.abs(run.electrolyte_concentration / 1000 - 1).max() for run in runs.values()):.1e}"
)
print(
    f"high conductivities: largest |V_DFN - V_SPM| = {1e3 * np.abs(limit['DFN'].terminal_voltage - limit['SPM'].terminal_voltage).max():.3f} mV over the 1C discharge"
)
print(
    f"{'C-rate':>6s} {'kappa':>6s} {'V(t1) [V]':>10s} {'V_end [V]':>10s} {'shift vs 1 S/m [mV]':>20s} {'one-third rule [mV]':>20s} {'ratio':>6s}"
)
for (kappa, rate), run in runs.items():
    shift = 1e3 * (runs[1.0, rate].terminal_voltage[1] - run.terminal_voltage[1])
    estimate = 1e3 * rate * one_c * (resistance(kappa) - resistance(1.0))
    print(
        f"{rate:6.1f} {kappa:6.1f} {run.terminal_voltage[1]:10.4f} {run.terminal_voltage[-1]:10.4f} {shift:20.1f} {estimate:20.1f} "
        f"{shift / estimate if estimate else 1.0:6.2f}"
    )

# ## Figure
#
# The discharge curves of all runs, and the ionic potential through the cell at the end of the 1C
# discharge for the three conductivities.

capacity = lambda rate, run: 5.0 * rate * run.times / 3600
fig = plots.figure(1, 2, size=(16, 6))
plots.line(
    y={
        f"{rate:g}C, κ = {kappa:g} S/m": (capacity(rate, run), run.terminal_voltage)
        for (kappa, rate), run in runs.items()
    },
    reference={
        "1C, SPM limit": (capacity(1.0, limit["SPM"]), limit["SPM"].terminal_voltage)
    },
    xlabel="discharged capacity [Ah]",
    ylabel="terminal voltage [V]",
    title="Discharge with a single-ion conductor",
    legend="lower left",
    ax=fig[0],
)
plots.line(
    y={
        f"κ = {kappa:g} S/m": (
            runs[kappa, 1.0].electrolyte_positions * 1e6,
            1e3
            * (
                runs[kappa, 1.0].electrolyte_potential[-1]
                - runs[kappa, 1.0].electrolyte_potential[-1][0]
            ),
        )
        for kappa in (1.0, 0.3, 0.1)
    },
    xlabel="position through the cell [µm]",
    ylabel="φ_e - φ_e(0) [mV]",
    title="Ionic potential at the end of the 1C discharge",
    legend="lower left",
    ax=fig[1],
)
plots.show()

# ## Going further
#
# Set $t_+$ back to the liquid value 0.26 at the same conductivity: the salt gradient adds the
# concentration overpotential and cuts the capacity at high rates. Thicker electrodes show where
# the low conductivity of solid electrolytes concentrates the reaction near the separator.